Description
Zinn Giessform Base, Steppe mit Schachtdeckel rund Alginat The molds were originally developed The molds were originally developed for the construction of cribs Processing time : 8 – 10 minutes Demoulding time: 20 – 100 minutes Density of the products: 1730 kg m³ Compressive strength: 25 – 30 MPa drying oven Flexural Strength Maximum Load: 18 MPa Expansion on setting: < 0 for events You will receive a new pewter mold made of heat resistant HB silicone rubber (up to 450 degrees Celsius briefly) for casting low melting metal alloys such as tin or lead